SL -NR. |
MATERIALEIGENSCHAFTEN
FÜR CARBON BLACK N375 |
U/M |
ZIEL
WERT |
MIN
WERT |
MAX
WERT |
TESTERGEBNISSE |
TESTMETHODE
ASTM -REF. |
1 | SPEZIFISCHES GEWICHT @ 25DEG C (TYPISCH) | K. A. | 1,800 | D-1817 | |||
2 | DBP -ABSORPTION | CC/100g | 114 | 109 | 119 | 113 | D-2414 |
3 | GIESSEN SIE DIE DESITÄT | Kg/m3 | 345 | 305 | 385 | 367 | D-1513 |
4 | JODZAHL | K. A. | 90 | 85 | 95 | 89 | D-1510 |
5 | LOSS,1 STUNDEN @ 125 DEG C (POLYBEUTEL ) ERHITZEN, WIE ERHALTEN | % | 2,5 | -- | D-1509 | ||
6 | LOSS,1 STUNDEN @ 125 DEG C ERHITZEN (POLYBEUTEL BULX), WIE EMPFANGEN. WIE ERHALTEN | % | 2,5 | 0,5 | D-1509 | ||
7 | RÜCKSTÄNDE AUF 45 -MIKROMETER -SIEB (US#325 -SIEB) | % | 0,1 | 0,02 | D-1514 | ||
8 | RÜCKSTÄNDE AUF 500 -MIKROMETER -SIEB (US#35 -SIEB) | % | 0,001 | 0,000 | D-1514 | ||
9 | 5' FEINFALLE DURCH 125 MIKROMETER SIEB (US#120 BILDSCHIRM)-BEUTEL | % | 12,0 | --- | D-1506 | ||
10 | 5' FEINKORNDMESSER ÜBER 125 MIKROMETER SIEB (US#120 SIEB)-LOSE | % | 6,0 | 5,1 | D-1506 | ||
11 | ZINN.% ITRB #3 | % | 114 | 109,0 | 119,0 | 110 | D-3265 |
12 | PELLETHÄRTE | gmf | 40 | 15 | 90 | 33 | D-3313/D-5203 |
13 | ASCHE | % | 0,5 | 0,3 | D-1506 | ||
14 | 24 M4 ZERQUETSCHTE DBP | CC/100g | 96 | 91 | 101 | 94 | D-3493 |
15 | STICKSTOFFOBERFLÄCHE | m2/g | 93 | 88 | 98 | 93 | D-4820 |
16 | GESAMTER SCHWEFELGEHALT | % | 2,0 | 1,1 | D-1691 | ||
17 | PH -WERT | 6,0 | 10 | 6,5 | D-1512 | ||
18 | TOLUOL -VERFÄRBUNG | % | 90 | 98 | D-1618 | ||
19 |
EIGENSCHAFT DES COMPOUNDERES :
ASTM-NR-NB D3192&3182, VERGLICHEN MIT IRB #7 300 % MOD (AUSGEHÄRTET 30' BEI 145 DEG.C) DUMBEL |
Mp3 | 0,1 | -1,5 | +1,7 | 0,2 | D-412 |