High Permeability Low Core Loss Nanocrystalline Core for Inverter Welding Machine

Model NO.
90/130*50MM
HS Code
85049019
Production Capacity
360 Tons/Year
Reference Price
$ 17.10 - 178.20

Product Description

High Permeability Low Core Loss Nanocrystalline Core For Inverter Welding Machine
 
Product Description
Features:            
    high saturation magnitical induction,minimize the volume of the transformer
    High permeability and low coercive force,increase the efficience of the transformer
    Low core loss,reduce the temperature rise of the transformer    
    Good temperature stability, can work under 130oC for long time    
             
Applications:            
    Various high frequency switching mode power supplies      
    inverter welding machine          
    x-ray power supplies,laser power supplies,communication power supplies  
    UPS,high frequency induction heating power supplies      
    charging power supplies          
    electrolytic plating power supplies etc.        
Detailed Photos

Core Winding:

High Permeability Low Core Loss Nanocrystalline Core for Inverter Welding Machine
Cores are annealing in vacuum furnace:
High Permeability Low Core Loss Nanocrystalline Core for Inverter Welding Machine High Permeability Low Core Loss Nanocrystalline Core for Inverter Welding Machine Cores are 100% tested after annealing:

High Permeability Low Core Loss Nanocrystalline Core for Inverter Welding Machine
Solidify for the cores:
High Permeability Low Core Loss Nanocrystalline Core for Inverter Welding Machine High Permeability Low Core Loss Nanocrystalline Core for Inverter Welding Machine High Permeability Low Core Loss Nanocrystalline Core for Inverter Welding Machine

Core Packing:
High Permeability Low Core Loss Nanocrystalline Core for Inverter Welding Machine High Permeability Low Core Loss Nanocrystalline Core for Inverter Welding Machine High Permeability Low Core Loss Nanocrystalline Core for Inverter Welding Machine
Product Parameters
Electrical property standard :  
   The comparison between nano crystalline core and ferrite core
bascal parameter nanocrystallie core  Ferrite core
Saturated magnetic induction Bs(T)( T )   1.25 0.5
Residual magnetic field density Br(T)( T ) ( 20KHz ) <0.20 0.2
core loss( 20KHz/0.5T ) ( W/Kg )   < 25 can not be used
core loss( 5 0KHz/0. 32 T ) ( W/Kg )   <35 can not be used
permeability ( 20KHz ) ( Gs/Oe ) >20,000 2,000  
coercive force (A/m)   <1.60 6
Saturated magnetostrictive coefficient
λs
(×10 -6 )  
<2 4  
Resistivity
( mW -cm)  
130 10 6  
Curie temperature ( ºC )   570 <200
S tacking factor 0.75 -
Packaging & Shipping

All cores are well packed by strpong plywood boxes to acoid any damage during transportation:
High Permeability Low Core Loss Nanocrystalline Core for Inverter Welding Machine

 

PNEUTEC.IT, 2023