Sample |
Appearance |
Density
(g/cm 3 @25 o C) |
Viscosity
(mPa·s@40 o C) |
Package Size
(kg/drum) |
HD-4060 |
Clear viscous liquid or waxy solid |
1.13~1.18 | 1900~2400 | 220 |
HD-1900 |
Colorless or pale yellow liquid |
1.18~1.20 | 400~700 | 235 |
Items | Unit | Value | Test Standard |
Density | g/cm 3 | 0.38-0.45 | GB/T 4472-2011 / DIN 53479 |
Hardness | Shore A | 40-50 | HG/T 2489-2007 / DIN 53505 |
Tensile Strength | MPa | >4 | GB/T 10654-2001 / DIN 53504 |
Elongation | % | >350 | GB/T 10654-2001 / DIN 53504 |
Angle tear strength | kN/m | >20 | GB/T 529-2008 / DIN ISO 34-1 |
Flexing | cycle | 100000 | HG/T 2411-2006 / DIN 53578 |
Abrasion | mm 3 | <200 | GB/T 9867-2008 / DIN 53516 |
Test Items | Unit | Value |
Ratio of (P+C) and I component | - | 100/88~90 |
Material temperature | o C | A:40~45 / B:38~42 |
Cream time | s | 8~10 |
End of rise time | s | 45~55 |
Pinch time | s | 100~120 |
Free rise density | / g/cm 3 | 0.25~0.28 |
Metal mold temperature | o C | 45~55 |
Demould time | min | 3~4 |