| Al | Mn | Fe | Ni | Si | Cu | C | Ti |
| 4.5-5.5 | Max 0.3 | Max 0.3 | Bal. | Max 0.5 | Max 0.08 | Max 0.005 | Max 0.3 |
| Density ( g/cm3 ) | 8.2 |
| Electrical resis t ivity at 2 0 ºC ( mm2/m ) | 0.42 |
| Coating Harness | Coating Strength | Deposit Rate | Deposit Efficiency | Machilityineab |
| 23-25 HRC | 65-68 Mpa | 10 lbs /hr/100A | 60-70% | Good |
| Specific heat capacity |
| Melting point ( ºC ) | 1 010 |
| Max continuous operating temperature in air ( ºC ) | 800 |
| Magnetic properties | non-magnetic |