Steel grade  | C  | Si  | Mn  | P  | S  | Cr  | Mo  | Ni  | Other elem ents  | |||||||
Steel name  | Steelnum ber  | min  | max  | min  | max  | min  | max  | max  | max  | min  | max  | min  | max  | min  | max  | |
E235  | 1.0308  | 0.17  | -  | 0.35  | -  | 1.20  | 0.030  | 0.035  | ||||||||
E275  | 1.0225  | 0.21  | -  | 0.35  | -  | 1.40  | 0.030  | 0.035  | ||||||||
E315  | 1.0236  | 0.21  | -  | 0.30  | -  | 1.50  | 0.030  | 0.035  | ||||||||
E355 b  | 1.0580  | 0. 22  | -  | 0.55  | -  | 1.60  | 0.030  | 0.035  | ||||||||
E470  | 1.0536  | 0.16  | 0.22  | 0.10  | 0.50  | 1.30  | 1.70  | 0.030  | 0.035  | Al min 0.010, N max. 0.020, Nb Max.0.07,V 0.08/0.15  | ||||||
C22E  | 1.1 151  | 0. 17  | 0. 24  | -  | 0. 40  | 0. 40  | 0. 70  | 0.0 35  | 0.0 35  | |||||||
C35E  | 1.1 181  | 0. 32  | 0. 39  | -  | 0. 40  | 0. 50  | 0. 80  | 0.0 35  | 0.0 35  | |||||||
C45E  | 1.1 191  | |||||||||||||||
| Term | Symbol | Explanation | 
| Cold-finished/hard (cold-finished as-drawn)  | BK | No heat treatment after the last cold-forming process. The tubes therefore have only low deformability. | 
| Cold-finished/soft (lightly cold-worked)  | BKW | After the last heat treatment there is a light finishing pass (cold drawing) With proper subsequent processing, the tube can be cold-formed (e.g. bent, expanded) within certain limits. | 
| Annealed | GBK | After the final cold-forming process the tubes are annealed in a controlled atmosphere or under vacuum. | 
| Normalized | NBK | The tubes are annealed above the upper transformation point in a controlled atmosphere or under vacuum. | 